Name the welding defect in which we observe a long and continuous visual separation line between the base metal and the heat affected zone. 

This question was previously asked in
SSC JE Mechanical 05 Jun 2024 Shift 2 Official Paper - 1
View all SSC JE ME Papers >
  1. Incomplete fusion
  2. Lamellar tearing
  3. Hot cracking 
  4. Undercut 

Answer (Detailed Solution Below)

Option 2 : Lamellar tearing
Free
RRB JE CBT I Full Test - 23
14.3 K Users
100 Questions 100 Marks 90 Mins

Detailed Solution

Download Solution PDF

Explanation:

Lamellar Tearing:

  • Lamellar tearing is a type of welding defect that occurs primarily in the base metal, parallel to the weld fusion boundary.
  • It is characterized by a long and continuous visual separation line, usually caused by tensile stresses acting perpendicular to the plane of rolled steel plates.

Causes:

  • Non-Metallic Inclusions: Lamellar tearing is often associated with the presence of non-metallic inclusions, such as sulfides and oxides, which are elongated during the rolling process of steel plates.
  • High Through-Thickness Strain: The defect typically occurs when high tensile stresses are applied in the through-thickness direction (perpendicular to the rolled layers of the plate).
  • Thermal Stresses: Differential heating and cooling during the welding process can induce thermal stresses in the material, contributing to the risk of lamellar tearing.

Visual Identification:

  • The defect manifests as a continuous or intermittent separation line parallel to the weld fusion boundary.
  • This line represents a lack of cohesion within the base metal, often visible on the surface and extending into the thickness of the plate.

Prevention:

  • Material Selection: Use materials with low sulfur content and low inclusion levels to reduce the risk of lamellar tearing.
  • Welding Techniques: Employ welding techniques that minimize through-thickness stresses, such as low heat input welding methods.
  • Design Considerations: Design joints to minimize restraint and avoid high through-thickness stresses.
Latest SSC JE ME Updates

Last updated on May 28, 2025

-> SSC JE ME Notification 2025 will be released on June 30. 

-> The SSC JE Mechanical engineering application form will be available from June 30 to July 21. 

-> SSC JE 2025 CBT 1 exam for Mechanical Engineering will be conducted from October 2 to 31. 

-> SSC JE exam to recruit Junior Engineers in different disciplines under various departments of the Central Government.

-> The selection process of the candidates for the SSC Junior Engineer post consists of Paper I, Paper II, Document Verification, and Medical Examination.

-> Candidates who will get selected will get a salary range between Rs. 35,400/- to Rs. 1,12,400/-.

-> Candidates must refer to the SSC JE Previous Year Papers and SSC JE Civil Mock Test, SSC JE Electrical Mock Test, and SSC JE Mechanical Mock Test to understand the type of questions coming in the examination.

Get Free Access Now
Hot Links: lotus teen patti teen patti gold teen patti circle teen patti master 51 bonus teen patti master gold download